Originally Posted by KJJames View Post
Pia, the COE is 90 and the annealing temp is 960 - 970. Now that is on the production colors. Remember, I am still new to this glass too. As I have been researching there are some odd lot colors such as the auroras which you want to anneal at around 930ish. Squid is the expert on that. Do an advanced search with bullseye and choose the tips, techniques and questions forum. You will come up with a lot of info. You will see some of the most beautiful work too.
You can anneal all of your glass in the 930 range - I do. Including 104 and 96.