Stick it in a kiln and let it get round on the edges. It also cooks the dichro coating. I find it much easier to work with. Ah, I think I have some photos. It may be difficult to see without zooming in but that's what I have available here.

I THINK slumping is around 1200 degrees. Someone correct me if I am wrong. I watch it closely because you don't want it to get too hot or it will turn into a thick round dot.

Put it in the kiln (on a kiln-washed shelf) dichro side down.