Quote:
Originally Posted by FosterFire View Post
Send me a PM and I will send you a free sample of FosterFire. The stuff they sell in the kit is enough to make a sane person cry. I sell on Etsy or also if you email me. I have 3 formulas. The best for beginners as a balance between cost and being hard to break is the Heavy Duty. If you plan to use presses then I would recommend the Smooth & Tuff.

If you want one that is really really really tough then I recommend Fusion which can be purchased from Frantz Art Glass. It's harder to get the beads off after words, just an FYI. And they don't do samples. Also: every bead release works better air dried.

You might see if there is a bead group in your area and if they're doing demos then you can try different releases.
Definitely interested in trying your bead release! I pmed you.