i have had problem with silver glass and pressing. i make the bead, encase it and then when i go to press in a brass press some weird poop develops that i can't deal with since it is under the encasement layer. BTY, thought i read something about brass presses being too cold and if you kept them warm maybe the poop wouldn't develop....so put them on the top of the chili pepper kiln and the things got so hot i couldn't touch them! opposite of the ice treatment. what do you all think about encased silver glass and the post press poop development?