Thank you. Your chart will be most helpful.
-BEP
Quote:
Originally Posted by Listenup
All of the beads in my chart were annealed @ 968°F and exposed to the direct flame of a HotHead torch (abt 1500°F). The powder is the outside layer on all my beads. Some survived, some didn't. The only way to be 100% certain it will survive your planned application is to design & run a test first.
|
__________________
Brian E. Parker aka BEPNewt
Lifelong glass lover, now getting to work with it. Using a Bravo on an M20 & Natural Gas ( inner ), Tanked O2 & Propane ( outer ).
Grew up near To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts. .
|