Lower your kiln temperature and lengthen the annealing time need to be done methodically - test it out 10F at a time. I have written about it in my blog of annealing silver glass if you are interested.

http://envisionsf.blogspot.com/2009/...mperature.html

Hope this helps.
__________________
Hayley


To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.


To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
|
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
|
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
|
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
|
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
Reply With Quote