THANK YOU for the annealing info and the bead sample pics! You do such nice work. It's inspirational.


Quote:
Originally Posted by veeanca View Post
Here are my experiments



The semi opaque white and pink went opaque because I annealed them at a too high temp. I have learnt since that devardi will keep its translucency (for the semi opaques) if annealed at a lower temp (490C). I was previously annealing at 500-510C and the lush semi opaques would go opaque.

The frogs are all effetre pea green. Only the base colours are devardi. I have been able to create an encased floral using a trans green moretti base, white moretti flowers with devardi trans pink on top, all fully encased in vetrofond clear with no cracks (but the bead turned out ugly so I won't post a pic of it )