You can also roll a bead in the powder. Go for a thin layer. Then case that. I had a hard time on my first attempt. I rolled it in a frit tray with a bunch of the powder piled up. The moisture in the powder heated so fast it burped steam out of the pile with a poof of powder. May not be a problem in dryer climates. I now put a small layer on a graphite pad and roll in it that way.